ERNiCrMo-4


Product Overview:

Excellent corrosion resistance in a wide range of corrosive media including, sulphur compounds and chloride ions.
Excellent resistance to pitting, crevice corrosion and stress corrosion cracking.
Withstands the corrosive effects of wet chlorine gas, hypochlorite and chlorine dioxide.
Good for sea water applications.


Key word:

Inconel | Hastelloy


MAIL: info@bh-alloy.com

MOB: +86-511-80269668

FEEDBACK

Product Details


Ernicrmo-4 welding wire is mainly used for welding Hastelloy C-276 alloy and other nickel chromium molybdenum alloys by tungsten inert gas shielded welding and molten gas shielded welding, and can also be used for surface surfacing of steel. This kind of welding material has excellent corrosion resistance in various corrosive media, which is the ability to resist pitting corrosion and crack corrosion.
This welding wire can be used for welding different materials, including Hastelloy C-276 alloy and other nickel alloys, stainless steel and low alloy steel.

 

Grade/Element ERNiCrMo-3 ERNiCrMo-4 ERNiCrFe-3 ERNiCr-3 ERNiCu-7 ERCuNi ERNi-1 ER385 ERNiCrMo-6 ERNiCrMo-10 ERNiFeCr-1 ERNiFeCr-2 ERNiCrFe-7 ERNiFe55
C ≤0.02 ≤0.02 ≤0.02 ≤0.5 ≤0.04 ≤0.03 ≤0.05 ≤0.025 ≤0.02 ≤0.015 ≤0.05 ≤0.08 ≤0.04 ≤0.1
Mn ≤0.4 ≤1.0 3.0-3.5 2.5-3.5 2.5-3.5 0.5-1.0 ≤0.9 1.0-2.0 2.0-4.0 ≤0.5 ≤1.0 ≤0.3 ≤1 ≤1.0
P ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01
S ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01
Si ≤0.15 ≤0.08 ≤0.20 ≤0.1 ≤0.15 ≤0.15 ≤0.5 ≤0.35 ≤0.2 ≤0.08 ≤0.5 ≤0.3 ≤0.5 ≤0.15
Cr 20-23 14.5-16 16-17 19-22 None ≤0.1 None 20-22 14-17 20-22.5 20-23.5 17-21 29-31.5  ≥55
Ni Remain Remain Remain Remain 64-69 30-32 Remain 24-26 Remain Remain 38-46 50-55 Remain None
Cu None None None None Remain Remain None 1.2-2.0 ≤0.3 None 1.5-3 None None None
Mo 8.5-10 15-17 None None None None None 4.2-5.2 7.0-9.0 12.5-14.5 2.5-3.5 2.8-3.3 None None
Ti ≤0.4 None ≤0.75 ≤0.7 1.5-3.0 ≤0.5 2.0-3.5 None None None 0.6-1.2 0.65-1.15 ≤1 None
Fe ≤1.0 4.0-7.0 ≤2.0 ≤2.0 ≤1.0 ≤0.65 None None ≤4.0 2-6 ≥22 Remain 7-11 Remain
Nb 3.15-4.15 None 2.0-2.5 2.0-3.0 None None None None 1.0-2.0 None None 4.5-5.5 None None
W None 3.0-4.5 None None None None None None 1.0-2.0 None None None None None
Impurities ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30

The above welding materials can produce TIG and MIG wire.

Production Specifications
TIG MIG MIG: 15KG/SPOOL
Axis: D300
TIG: 5KG/BOX
Axis: D300
Φ1.6*1000 Φ0.8
Φ2.0*1000 Φ1.0
Φ2.4*1000 Φ1.2
Φ4.0*1000 Φ1.6

 

 

Designations: AWS 054

 

Specifications: ASTM B574
ASTM B575
ASTM B619

 

Alloy Details

Density Melting Point Coefficient of Expansion Modulus of Rigidity Modulus of Elasticity
8.89 g/cm³ 1370 °C 11.2 μm/m °C (20 – 100 °C) 78.6 kN/mm² 205.5 kN/mm²
0.321 lb/in³ 2500 °F 6.2 x 10-6 in/in °F (70 – 212 °F) 11400 ksi 29806 ksi

 

Heat treatment of finished parts

Condition as supplied by AWI Type Temperature Time Cooling
Annealed or Spring Temper Stress Relieve 400 – 450 °C (750 – 840 °F) 2 Hr Air

 

Properties

Annealed    
Approx. tensile strength <1050 N/mm² <152 ksi
Approx. operating temperature depending on loading and environment -200 to +400 °C -330 to +750 °F

 

Spring Temper    
Approx. tensile strength 1300 – 1700 N/mm² 189 – 247 ksi
Approx. operating temperature depending on loading and environment -200 to +400 °C -330 to +750 °F

 

The above information is typical. If you require different please ask.

Advantages

Specialized

Focus on creating product value for customers.

Quality

Create a quality enterprise and establish a reputation.

Technology

Manufacture with heart, achieve quality.

Service

Excellent service, exceeding customer expectations.

Raw Materials

Nickel Plate


Nickel Plate

Pure Iron


Pure Iron

Electrolytic Manganese


Electrolytic Manganese

Sponge Titanium


Sponge Titanium

Metal Chrome


Metal Chrome

Production Ability