ERNiCu-7


Product Overview:

Excellent corrosion resistance in a wide range of acidic & alkaline environments
Especially suitable for reducing conditions
Good ductility & thermal conductivity
Good for sea water applications


Key word:

Inconel | Hastelloy


MAIL: info@bh-alloy.com

MOB: +86-511-80269668

FEEDBACK

Product Details


ERNiCu-7 is a copper-nickel alloy base wire for GMAW and GTAW welding of Monel alloys 400 and 404. Also used for overlaying steel.

 

Grade/Element ERNiCrMo-3 ERNiCrMo-4 ERNiCrFe-3 ERNiCr-3 ERNiCu-7 ERCuNi ERNi-1 ER385 ERNiCrMo-6 ERNiCrMo-10 ERNiFeCr-1 ERNiFeCr-2 ERNiCrFe-7 ERNiFe55
C ≤0.02 ≤0.02 ≤0.02 ≤0.5 ≤0.04 ≤0.03 ≤0.05 ≤0.025 ≤0.02 ≤0.015 ≤0.05 ≤0.08 ≤0.04 ≤0.1
Mn ≤0.4 ≤1.0 3.0-3.5 2.5-3.5 2.5-3.5 0.5-1.0 ≤0.9 1.0-2.0 2.0-4.0 ≤0.5 ≤1.0 ≤0.3 ≤1 ≤1.0
P ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01
S ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01 ≤0.01
Si ≤0.15 ≤0.08 ≤0.20 ≤0.1 ≤0.15 ≤0.15 ≤0.5 ≤0.35 ≤0.2 ≤0.08 ≤0.5 ≤0.3 ≤0.5 ≤0.15
Cr 20-23 14.5-16 16-17 19-22 None ≤0.1 None 20-22 14-17 20-22.5 20-23.5 17-21 29-31.5  ≥55
Ni Remain Remain Remain Remain 64-69 30-32 Remain 24-26 Remain Remain 38-46 50-55 Remain None
Cu None None None None Remain Remain None 1.2-2.0 ≤0.3 None 1.5-3 None None None
Mo 8.5-10 15-17 None None None None None 4.2-5.2 7.0-9.0 12.5-14.5 2.5-3.5 2.8-3.3 None None
Ti ≤0.4 None ≤0.75 ≤0.7 1.5-3.0 ≤0.5 2.0-3.5 None None None 0.6-1.2 0.65-1.15 ≤1 None
Fe ≤1.0 4.0-7.0 ≤2.0 ≤2.0 ≤1.0 ≤0.65 None None ≤4.0 2-6 ≥22 Remain 7-11 Remain
Nb 3.15-4.15 None 2.0-2.5 2.0-3.0 None None None None 1.0-2.0 None None 4.5-5.5 None None
W None 3.0-4.5 None None None None None None 1.0-2.0 None None None None None
Impurities ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30 ≤0.30

The above welding materials can produce TIG and MIG wire.

Production Specifications
TIG MIG MIG: 15KG/SPOOL
Axis: D300
TIG: 5KG/BOX
Axis: D300
Φ1.6*1000 Φ0.8
Φ2.0*1000 Φ1.0
Φ2.4*1000 Φ1.2
Φ4.0*1000 Φ1.6

 

Designations: AWS 040

 

Specifications: AMS 4730,ASTM B164

 

Alloy Details

Density Melting Point Coefficient of Expansion Modulus of Rigidity Modulus of Elasticity
8.8 g/cm³ 1350 °C 13.9 μm/m °C (20 – 100 °C) 65.3 kN/mm² 173 kN/mm²
0.318 lb/in³ 2460 °F 7.7 x 10-6 in/in °F (70 – 212 °F) 9471 ksi 25092 ksi

 

Heat treatment of finished parts

Condition as supplied by AWI Type Temperature Time Cooling
Annealed or Spring Temper Stress Relieve 300 – 320 °C
(570 – 610 °F)
0.5 – 1 Hr Air

 

Properties

Annealed    
Approx. tensile strength <600 N/mm² <87 ksi
Approx. operating temperature -200 to +230 °C -330 to +445 °F

 

Spring Temper    
Approx. tensile strength 800 – 1100 N/mm² 116 – 160 ksi
Approx. operating temperature -200 to +230 °C -330 to +445 °F


 

The above information is typical. If you require different please ask.

Previous

Next

Previous

Next

Advantages

Specialized

Focus on creating product value for customers.

Quality

Create a quality enterprise and establish a reputation.

Technology

Manufacture with heart, achieve quality.

Service

Excellent service, exceeding customer expectations.

Raw Materials

Nickel Plate


Nickel Plate

Pure Iron


Pure Iron

Electrolytic Manganese


Electrolytic Manganese

Sponge Titanium


Sponge Titanium

Metal Chrome


Metal Chrome

Production Ability