Hastelloy C-22


Product Overview:

Better overall corrosion resistance than Hastelloy C-4 & C-276 and Inconel 625.
Outstanding resistance to pitting, crevice corrosion and stress corrosion cracking.

Category:


Key word:

Inconel | Hastelloy


MAIL: info@bh-alloy.com

MOB: +86-511-80269668

FEEDBACK

Product Details


Element Min % Max %
Cr 20.00 22.50
Mo 12.50 14.50
Fe 2.00 6.00
W 2.50 3.50
C 0.015
Si 0.08
Co 2.50
Mn 0.50
V 0.35
P 0.02
S 0.02
Ni bal

 

Designations: AWS 053

 

Specifications: ASTM B574,ASTM B575,ASTM B619

 

Alloy Details

Density Melting Point Coefficient of Expansion Modulus of Rigidity Modulus of Elasticity
8.69 g/cm³ 1399 °C 12.4 μm/m °C (20 – 100 °C) 78.6 kN/mm² 205.5 kN/mm²
0.314 lb/in³ 2550 °F 6.9 x 10-6 in/in °F (70 – 212 °F) 11400 ksi 29806 ksi

 

Heat treatment of finished parts

Condition as supplied by AWI Type Temperature Time Cooling
Annealed or Spring Temper Stress Relieve 400 – 450 °C (750 – 840 °F) 2 Hr Air

 

Properties

Annealed    
Approx. tensile strength <1100 N/mm² <159 ksi
Approx. operating temperature depending on loading and environment -200 to +400 °C -330 to +750 °F

 

Spring Temper    
Approx. tensile strength 1400 – 1700 N/mm² 203 – 247 ksi
Approx. operating temperature depending on loading and environment -200 to +400 °C -330 to +750 °F

The above information is typical. If you require different please ask.

Advantages

Specialized

Focus on creating product value for customers.

Quality

Create a quality enterprise and establish a reputation.

Technology

Manufacture with heart, achieve quality.

Service

Excellent service, exceeding customer expectations.

Raw Materials

Nickel Plate


Nickel Plate

Pure Iron


Pure Iron

Electrolytic Manganese


Electrolytic Manganese

Sponge Titanium


Sponge Titanium

Metal Chrome


Metal Chrome

Production Ability