Inconel 718
Product Overview:
Higher strength than Inconel X-750
Better mechanical properties at lower temperatures than Nimonic 90 & Inconel X-750
Age hardenable
High temperature dynamic applications
Category:
Key word:
Inconel | Hastelloy
FEEDBACK
Product Details
Element | Min % | Max % |
C | – | 0.08 |
Mn | – | 0.35 |
Si | – | 0.35 |
P | – | 0.015 |
S | – | 0.015 |
Cr | 17.00 | 21.00 |
Ni | 50.00 | 55.00 |
Mo | 2.80 | 3.30 |
Nb/Cb | 4.75 | 5.50 |
Ti | 0.65 | 1.15 |
Al | 0.20 | 0.80 |
Co | – | 1.00 |
Ta | – | 0.05 |
B | – | 0.006 |
Cu | – | 0.30 |
Pb | – | 0.0005 |
Bi | – | 0.00003 |
Se | – | 0.0003 |
Fe | bal | – |
The above welding materials can produce TIG and MIG wire.
Production Specifications
TIG | MIG | MIG: 15KG/SPOOL Axis: D300 |
TIG: 5KG/BOX Axis: D300 |
Φ1.6*1000 | Φ0.8 | ||
Φ2.0*1000 | Φ1.0 | ||
Φ2.4*1000 | Φ1.2 | ||
Φ4.0*1000 | Φ1.6 |
Designations: AWS 013
Specifications: AMS 5662,AMS 5663,AMS 5832,AMS 5962,ASTM B637
Alloy Details
Density | Melting Point | Coefficient of Expansion | Modulus of Rigidity | Modulus of Elasticity |
8.19g/cm³ | 133 6 °C | 13.0 μm/m °C (20 – 100 °C) | 77.2 kN/mm² | 204.9 kN/mm² |
0.296 lb/in³ | 2437 °F | 7.2 x 10-6 in/in °F (70 – 212 °F) | 11197 ksi | 29719 ksi |
Heat treatment of finished parts
Condition as supplied by AWI | Type | Temperature | Time | Time |
No. 1 or Spring Temper | Anneal Age Harden Total Age |
980 °C (1800 °F) 720 °C (1330 °F) 620 °C (1150 °F) |
1hr 8hr 18hr |
Air Furnace Air |
No. 1 or Spring Temper (for ISO 15156-3 / NACE MR 0175) |
Anneal Age Harden |
1010 °C (1850 °F) 790 °C (1455 °F) |
2hr 6hr |
Air Air |
No. 1 Temper or Spring Temper | Age Harden Total Age |
720 °C (1330 °F) 620 °C (1150 °F) |
8hr 18hr |
AirFurnace Air |
Properties
Annealed | ||
Approx. tensile strength | <1000 N/mm² | <145 ksi |
No. 1 Temper | ||
Approx. tensile strength | 1000 – 1200 N/mm² | 145 – 175 ksi |
Spring Temper | ||
Approx. tensile strength | 1250 – 1550 N/mm² | 180 – 225 ksi |
No. 1 Temper + Annealed + Aged | ||
Approx. tensile strength | 1250 – 1450 N/mm² | 181 – 210 ksi |
Approx. operating temperature depending on loading and environment | -200 to +550 °C | -330 to +1020 °F |
No. 1 Temper + Aged | ||
Approx. tensile strength | 1520 – 1720 N/mm² | 220 – 250 ksi |
Approx. operating temperature depending on loading and environment | Contact Alloy Wire Technical Dept |
Spring Temper + Annealed + Aged | ||
Approx. tensile strength | 1250 – 1450 N/mm² | 181 – 210 ksi |
Approx. operating temperature depending on loading and environment | -200 to +550 °C | -330 to +1020 °F |
Spring Temper + Aged | ||
Approx. tensile strength | 1700 – 1950 N/mm² | 247 – 283 ksi |
Approx. tensile strength | Contact Alloy Wire Technical Dept |
The above information is typical. If you require different please ask.
Previous
Next
Previous
Next
Advantages
Specialized
Focus on creating product value for customers.
Quality
Create a quality enterprise and establish a reputation.
Technology
Manufacture with heart, achieve quality.
Service
Excellent service, exceeding customer expectations.
Raw Materials
Nickel Plate
Pure Iron
Electrolytic Manganese
Sponge Titanium
Metal Chrome
Related Products
Jiangsu Bohang Alloy Technology Co., Ltd.
MAIL: info@bh-alloy.com
ADD.:No. 8, Fenglin Avenue, East Park, Lvcheng Town, Danyang City, Jiangsu Province
Copyright© 2022 Jiangsu Bohang Alloy Technology Co., Ltd. Powered by www.300.cn
This website already supports IPV6 SEO